[Performance Characteristics]
 
 
166 Transparent Stone Adhesive is bicomponent, room temperature curing modified epoxy adhesive. The adhesive has transparent layer and has advantages of high adhesive strength, good water resistance, low stress, abrasion resistance, acid and alkali resistance, aging resistance and good cold & hot alternation
 
 
 
[Technical Parameters]
 
NO.
Item
Technical indicators
Appearance
Component A
Component B
Colorless or slightly yellow transparent viscous liquid
2
Viscosity(mPa·s)
Component A
30000~50000
Component B
8000~15000
3
Density(g/cm3)
A组份
Component A
1.05
Component B
0.99
4
Adhesive Mixing Ratio (A:B)
1∶1
5
Gel time (25℃,min)
10~15
6
Preliminary Curing Time (25℃,h)
1~1.5
7
Tensile Shear Strength (Steel-Steel, MPa)
≥10
 
 
 
[Scope of Application]
 
The product is applicable for bonding and repairing of stone and bedplate edges, which also has good bonding effect on ceramics, metals and concrete.
 
 
[Method of Application]
 
1. Clean, dry and remove dust, oil from the bonding parts;
 
2. Mix the adhesive evenly according to the specified proportion, use a adhesive mixing knife to apply adhesive to the stone bonding parts and press the bonding parts. At room temperature(over 25℃), the stone can be put into the next process after 24-hour’s curing; at low temperatures in winter(below 15℃), after the cured stone is heated to 50-60 ℃ and laid for 1-2 hours, the stone can be put into next process.
 
3. Add special toner into the adhesive according to the different colors of stones and adjust it into a color similar to that of the stone; the largest adding volume of toner is 5‰ of adhesive amount.
 
4. Use a cloth dipped with a small amount of alcohol or acetone to scrub the excessive adhesive squeezed out of the bonding parts before curing.
 
 
[Cautions]
 
1. The application temperature should not be less than 5℃; the adhesive can be heated appropriately in winter, to increase the temperature of stone surface.
 
2. As the adhesive should be used immediately after mixing, avoid mixing excessive adhesive at one time. The mixed adhesive must be used within the available time and the adhesive with gel should not be used. The higher the adhesive mixing temperature is and the more the adhesive amount is, the shorter the available time will be; whereas, the available time will be longer.
 
3. The apparatuses used to take Component A and Component B of the adhesive must not be mixed up; the remaining mixed adhesive must not be put into the tube again. The stone should not be removed before it is fully cured.
 
4. If it is not convenient to use the adhesive due to the high viscosity of adhesive liquid, the adhesive can be diluted by adding 3% ethanol or acetone or heated in 40-60 ℃ water to reduce its viscosity.
 
5. Because of the different physical, chemical nature of stone, please test the product experimently in advance to avoid errors! Do not mix up the lids of adhesive, fasten the lids after application and do not eat the adhesive by mistake!
 
 
 
Package and transportation
 
 
1. The product shall be kept in cool, dry and ventilating warehouse. Its service life is 1 year from its production date and may be put into use upon passing the examination after its expiry date.
 
2. The product belongs to general dangerous items. Please keep it away from heat source, fire source, sun burning, and rain during its transportation. Please handle it gently and avoid rolling, bumping, heavy pressing, upside down and side-placing during its transportation and loading.  
 
3. Packing specification: 2 kg/ set (18 kg/ item), Plastic bottle package.
 
4. Product standard: Q/BUEZ 026—2009